Key principles.
Below -40°C
Most carbon steels brittle below -40°C. Specify low-temperature grades or alternative materials.
Excellent
304/316L stainless retain ductility to -196°C. Standard cryogenic structural material.
Strengthens
Aluminum gains strength at low temperature. Excellent cryogenic performance.
Excellent
Copper, brass excellent at cryogenic temperatures. OFE copper standard for liquid hydrogen service.
Glass transition
Plastics become brittle below glass transition (Tg). Most engineering plastics: -40 to -60°C limit.
Specialty
Standard rubber stiffens. Use cryogenic-rated elastomers (silicone, fluorosilicone). Or metal seals.
FAQ
LNG -162°C: 9% nickel steel, austenitic stainless. Common LNG infrastructure materials.
-196°C: 304/316L stainless, aluminum 5083, OFE copper. Common materials.
-253°C: very specific materials. OFE copper, austenitic stainless, aluminum 5083.
Charpy V-notch impact at service temperature. Materials must meet minimum energy requirements.
Use matching low-temperature filler. Post-weld heat treatment per code. Charpy testing of weld required.
Yes — design for thermal expansion/contraction during cooldown. Insulation prevents condensation and frost damage.
Get an instant quote
Send your CAD — we reply with detailed pricing, lead time, and DFM feedback within 4 working hours.
Talk to an engineer
WhatsApp our team directly. Most messages answered within 12 minutes during work hours.
Explore all services
CNC, 3D printing, injection molding, sheet metal, casting, finishing — one quality system, one partner.
Working on a live project? Send the STEP file and the two or three features you are unsure about — an engineer replies with DFM notes and a price, usually within four working hours.